After a crap-ton of research I ordered the various silicones, catalysts, clay and coloring from Polytek in Easton, Pennsylvania. To keep the mold from sticking I used Polytek 2500 (a spray mold release that works with the chemical composition of the type of material I was using.)tripplec wrote: ↑Wed Oct 03, 2018 9:23 amThe beads are for alighnment, then you poor the silicone in and squeeze them together? Where did you get the materials, most things like sulferless clay are unheard of in Coos Bay Oregon. When you poored the second half, did you sprinkle in something like baby powder to to keep the halves from sticking?
Thanks guys for your positive comments. I'm going to continue messing around with different shore hardnesses of silicone casting material to see what works best. This one does fit the HW reg though.